ND Industries 240 Structural Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries 240 Structural Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent impact and solvent resistance
Physical Properties Metric English Comments
Viscosity 15000 cP
15000 cP
Thixotropic
Mechanical Properties Metric English Comments
Shear Strength 20.7 MPa
3000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 163 °C
325 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 0.333 - 1.00 min
0.00556 - 0.0167 hour
With Excel 600392 primer (Fixture)
1440 min
24.0 hour
With Primer (Full)
Descriptive Properties Value Comments
Color Amber
Curing Mechanism Excel Activator
Gap Fill, in. 0.5