Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 260 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 260 cP

@Temperature 30.0 °C
260 cP

@Temperature 86.0 °F
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Viscosity 260 cP

@Temperature 30.0 °C
260 cP

@Temperature 86.0 °F
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
Viscosity 260 cP

@Temperature 30.0 °C
260 cP

@Temperature 86.0 °F
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
Viscosity 260 cP
260 cP
DuPont Performance Polymers Hypalon® CP-826 Adhesion Primer, General Description  (discontinued **)
Hypalon CP 826 is a chlorinated, maleic anhydride grafted polypropylene resin.Suggested End Uses: Adhesion primer for:PolypropylenePolypropylene blends with TPOs (auto bumpers)Polyurethane foam, (at..
Copyright © lookpolymers.com All Rights Reserved