Thermal Properties Metric English Comments
Glass Transition Temp, Tg 39.0 - 46.0 °C
102 - 115 °F
ASTM E1545-00
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Glass Transition Temp, Tg 39.0 - 46.0 °C
102 - 115 °F
UV Postcure; ASTM E1545-00
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
Glass Transition Temp, Tg 42.0 - 46.0 °C
108 - 115 °F
ASTM E1545-00
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin
DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts ..
Glass Transition Temp, Tg 39.0 - 46.0 °C
102 - 115 °F
ASTM E1545-00
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..