Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 66.0 - 67.0 µm/m-°C @Temperature -40.0 - 0.000 °C |
36.7 - 37.2 µin/in-°F @Temperature -40.0 - 32.0 °F |
ASTM E831-00 |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
CTE, linear | 60.0 - 67.0 µm/m-°C @Temperature -40.0 - 0.000 °C |
33.3 - 37.2 µin/in-°F @Temperature -40.0 - 32.0 °F |
UV Postcure; ASTM E831-05 |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
CTE, linear | 66.0 - 67.0 µm/m-°C @Temperature -40.0 - 0.000 °C |
36.7 - 37.2 µin/in-°F @Temperature -40.0 - 32.0 °F |
ASTM E831-00 |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |