Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Innovene 1088 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: General purposeTypical applications: Water quenched blown filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fr.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.468 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.275 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | UV Postcure; ASTM D256A |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05H-01 Polypropylene Homopolymer Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. T.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Amoco® 6361 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.. |