Mechanical Properties Metric English Comments
Modulus of Elasticity 2.65 - 2.88 GPa
384 - 418 ksi
ASTM D638M
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Modulus of Elasticity 2.65 - 17.9 GPa
384 - 2600 ksi
Average value: 8.32 GPa Grade Count:124
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 2.65 - 2.88 GPa
384 - 418 ksi
UV Postcure; ASTM D368M
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
Modulus of Elasticity 2.65 - 2.88 GPa
384 - 418 ksi
ASTM D638M
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
Modulus of Elasticity 2.65 - 7.58 GPa
384 - 1100 ksi
Average value: 4.13 GPa Grade Count:16
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..