Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 39.0 - 46.0 °C | 102 - 115 °F | ASTM E1545-00 |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Glass Transition Temp, Tg | 39.0 °C | 102 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5690 Petroleum Hydrocarbon Resin Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and polyolefins. Information provid.. |
|||
Glass Transition Temp, Tg | 39.0 - 46.0 °C | 102 - 115 °F | UV Postcure; ASTM E1545-00 |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Glass Transition Temp, Tg | 39.0 - 46.0 °C | 102 - 115 °F | ASTM E1545-00 |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |