Mechanical Properties Metric English Comments
Flexural Modulus 2.04 GPa
296 ksi
ISO 178
PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66)
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o..
Flexural Modulus 2.04 GPa
296 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 4251R PPC+PC
High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors.
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880...
Flexural Modulus 2.04 - 2.37 GPa
296 - 344 ksi
ASTM D790M
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Flexural Modulus 2.04 GPa
296 ksi
Kuraray SEPTON® CM1 Compatibilizer
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC
LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Flexural Modulus 2.04 GPa
296 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10
LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant.
Flexural Modulus 2.04 GPa
296 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10
LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.04 GPa
296 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific)
Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.04 GPa
296 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific)
Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP (Asia Pacific)
LNP* Thermocomp* MB006HS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP
LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare.
Flexural Modulus 2.04 - 2.37 GPa
296 - 344 ksi
UV Postcure; ASTM D790M
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
Flexural Modulus 2.04 - 2.37 GPa
296 - 344 ksi
ASTM D790M
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
Flexural Modulus 2.04 GPa
296 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS VP-11 ELG
Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
Braskem H 501 HC Bioriented Film Polypropylene
Applications: High stiffness; barrier films for conversionInformation provided by Braskem
Flexural Modulus 2.04 GPa
296 ksi
1% secant; ASTM D790
Braskem H 501 HC Injection Molding Polypropylene
Description: H 501HC is a low melt flow rate homopolymer, designed for very high stifness aplications with good processability. This product exhibit excellent chemical resistance and barrier propert..