Material Notes:
Features: Alkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGeneral purposeGrease resistantLow moisture absorptionOil resistantResilientHigh rigiditySolvent resistantHigh strengthGood thermal stabilityGood toughnessInjection moldingForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.16 %
0.16 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
0.125 in; ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
0.125 in; ASTM D955
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Strength 91.7 MPa
13300 psi
ASTM D790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
0.125 in; ASTM D256
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
Type S; ASTM D1822
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ASTM D648