Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D1822 |
Network Polymers NPP Nylon 66G13L Description: NylonInformation provided by Network Polymers Inc. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D1822 |
Network Polymers Nylon 66G33L Description: Black NylonInformation provided by Network Polymers Inc. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | Type S; ASTM D1822 |
Chase Plastics CP Pryme® AC100 Acetal Copolymer Features: Alkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGeneral purposeGrease resistantLow moisture absorptionOil resistantResilientHigh rigiditySolv.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE) Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AD60-007 Blow Molding Resin Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 7140 Rigid PVC, Extrusion & Molding Georgia Gulf 7140 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 9275J Amber 05 Rigid PVC, Molding, Amber 05 Georgia Gulf 9275J Amber 05 is used for injection blow molded packages in cosmetic and toiletry applications. It is a pre-colored amber compound and all ingredients are FDA approved.Information pro.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 9275J Clear 40 Rigid PVC, Molding, Clear 40 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 8150 Rigid PVC, Extrusion & Molding Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 3240 Rigid PVC, Extrusion Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe.. |
|||
Tensile Impact Strength | 126 kJ/m² | 60.0 ft-lb/in² | ASTM D-1822 |
Axiall 3650 Rigid PVC, Extrusion Georgia Gulf 3650 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resistan.. |