Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.018 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® CE2055 NC010 PBT  (Unverified Data**)
Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Celanese Celcon® LW90 POM, Tribological  (Unverified Data**)
Celcon® LW90 is a nominal 9 melt flow rate based material specifically formulated for high speed, low wear applications against metals. LW90 conforms to applicable FDA regulations governing food co..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Celcon® WR25Z POM, UV Resistant  (Unverified Data**)
Celcon® WR25Z is a 2.5 nominal melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications. Celcon® WR25Z is a lower flow product ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® C 13021 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flowInformation provided by Celanese
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® C 27021 AS POM, Specialty  (Unverified Data**)
POM copolymerAntistatic grade, easy flowInformation provided by Celanese
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® C 36021 POM  (Unverified Data**)
Hostaform® C 36021 is an unfilled acetal copolymer grade formulated for high flow while retaining a good balance of mechanical properties.High flow, unfilled, for fast cycle & thin wallsInformation..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® C 52021 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with extremely high flowInformation provided by Celanese
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® MT24U01 POM, Medical Technology  (Unverified Data**)
Hostaform® MT24U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT24U01 is a low melt viscosity for fast cycli..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
LATI
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
Eurotec
Eurotec® Tecodur® PB70 NL IM PBT, unfilled, impact modified, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-27 TF10 Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
60x60x4; ISO 294-4
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM
30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® S 27063 XAP2® POM
Description: Easy flowing elastomer-containing injection molding type based on HOSTAFORM C 27021; with higher impact strength and reduced emissions. Burning rate ISO 3795 and FMVSS 302 < 100 mm/min ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored
Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Celanese Celcon® LM90 Acetal Copolymer (Capable of being Laser Marked)
Description: Celcon LM90 is a 9.0 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Celcon LM90 can be laser marked with barcodes, ID numbers..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Celcon® M25 POM  (Unverified Data**)
Celcon® acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Standard extrude..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® C 13021 RM POM, Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flow, with improved friction propertiesInformation provided by Celanese
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored
High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Celanese Celcon® M25N Acetal Copolymer
Description: Celcon acetal copolymer grade M25N is a high molecular weight, higher toughness and impact resistance nucleated grade primarily used for extrusion and selected injection molding applica..
Copyright © lookpolymers.com All Rights Reserved