Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa

@Thickness 3.17 mm
8900 psi

@Thickness 0.125 in
ASTM D638
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 61.4 MPa

@Thickness 3.17 mm
8900 psi

@Thickness 0.125 in
ASTM D638
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Spartech Royalite R6000 FR-PC Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Techmer ES Luriblend® POM CO TX10 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%) and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS 88 GF 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Styron EMERGEâ„¢ 4800-10 Polycarbonate
EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Styron EMERGEâ„¢ 4850-10 Polycarbonate
EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Styron EMERGEâ„¢ 4850-19 Polycarbonate
EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
Tensile Strength, Yield 61.4 MPa
8900 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 893-10 Polycarbonate
CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
Tensile Strength, Yield 61.4 MPa
8900 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 893-20 Polycarbonate
CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Styron EMERGEâ„¢ 4800-19 Polycarbonate
EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Chase Plastics CP Pryme® A100HF ABS
Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Chase Plastics CP Pryme® AC100 Acetal Copolymer
Features: Alkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGeneral purposeGrease resistantLow moisture absorptionOil resistantResilientHigh rigiditySolv..
Tensile Strength, Yield 61.4 MPa
8900 psi
Tra-Con Tra-Cast 3357 High Temperature Rigid Epoxy Casting System
TRA-CAST 3357 is a smooth pouring, low viscosity casting resin system recommended for rigid, large mass potting, encapsulating, laminating, filament-winding and coil embedment applications where the..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Omni Plastics OmniTuff™ CPP GRC20 Copolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.