Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.022 - 0.026 cm/cm | 0.022 - 0.026 in/in | ASTM D955 |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walledKepital® is a registered trademark of Korea .. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.026 cm/cm | 0.022 - 0.026 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX LMX171 PPO/PBT (Europe-Africa-Middle East) Noryl LMX171 is a PPO/PBT blend including conductive agent with a balanced heat/impact property profile. Noryl LMX differentiate from Noryl GTX by a lower moisture uptake (0.15%).This data was suppl.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190B Acetal General purpose reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. Black. Available in UV stabilized grades: R190-B2 (good weatherability); R190-H2B (maximum weatherab.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190H2-B Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized with carbon black for outstanding weatherability.Data provided by the manufacturer |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, Conditioned Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190H Acetal General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3.. |