Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Water Absorption 1.5 - 2.5 %
1.5 - 2.5 %
ISO 62
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0050 - 0.012 cm/cm
0.0050 - 0.012 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 131 MPa
19000 psi
ISO 2039-1
Tensile Strength at Break 156 MPa
22600 psi
ISO 527
Elongation at Break 2.2 %
2.2 %
ISO 527
Tensile Modulus 12.8 GPa
1860 ksi
ISO 527
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 125 °C
257 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V
550 V
CTI 100; IEC 112