Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 925-20PF Nylon 12, PTFE Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, PTFE Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 925-20PF Nylon 12, PTFE Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% filled PTFE lubricated, Nylon 12.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
ASTM D570
Linear Mold Shrinkage 0.017 cm/cm
0.017 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ATSM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 180 °C
356 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved