Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.018 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® MT8U05 POM, Medical Technology  (Unverified Data**)
Hostaform® acetal copolymer grade MT8U05 is a special grade developed for medical industry applications containing low residual monomers and no animal products. The material can be identified by U..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66  (Unverified Data**)
Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66
PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.018 - 0.0205 cm/cm
0.018 - 0.0205 in/in
LATI Latilub 75/4-20T PBT, PTFE Filled
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Teknor Apex Medalist® MD-165 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
DIS 294-4
Wellman Wellamid® 22LHI4 XE-GY1 Nylon 66, Impact Modified
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66
Description: Mineral Reinforced, Toughened Grade Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6
Description: Lubricated, Nucleated, Unfilled Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO DIS 294-4
Wellman Wellamid® XT1816-BK1 Toughened Nylon 66
Description: Toughened Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 3.20 mm
0.018 in/in

@Thickness 0.126 in
Unitika A1030TF PA6, Dry
Lubricating nylonInformation provided by Unitika Ltd.
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified
POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Celanese Celcon® GC15 POM, 15% Glass Reinforced  (Unverified Data**)
Celcon® GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.15% glass fibers, coupled for improved stiffnessStandard reciprocating sc..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Celanese Celcon® M140 POM  (Unverified Data**)
Celcon® acetal copolymer grade M140 is a moderately high flow general purpose injection molding grade. It is designed for use in applications requiring some enhanced flow characteristics over the s..
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Ashley Polymers Ashlene® RH190H Acetal
General purpose reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated RH190H-..
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..