Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 165 °C | 329 °F | ISO 11357-1 |
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•.. |
|||
Melting Point | 165 °C | 329 °F | |
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Melting Point | 165 °C | 329 °F | ASTM D4591 |
3M Dyneon™ THV 510ESD Fluorothermoplastic
(discontinued **) THV 510ESD is a flexible, fluoroplastic compound composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature proces.. |
|||
Melting Point | 165 - 190 °C | 329 - 374 °F | Huntsman/TMA |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 165 °C | 329 °F | (10°C/min); ISO 11357-1,2,3 |
Aardvark Polymers AARTEL® 800 Rotational Molding Resin Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of st.. |
|||
Melting Point | 165 °C | 329 °F | ASTM D789 |
KEP Kepital® F30 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | 165 - 188 °C | 329 - 370 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 165 °C | 329 °F | |
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 165 °C | 329 °F | ISO 11357 |
Polyram RamTal PM3009G4 Polyacetal for Injection Molding, 20% Glass Fiber Reinforced 20% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Total PPC 5660 Propylene, Heterophasic Copolymer ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application.. |
|||
Melting Point | 165 °C | 329 °F | DSC |
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applicat.. |
|||
Melting Point | 165 °C | 329 °F | DSC |
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating Process Stability TOTAL Petrochemicals Polypropylene 3866 features excellent processability and gas fade resistance.FDA. 3866 complies with all applicable FDA regulations for food contact applicat.. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Total PPH 5042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 5042 is homopolymer.ApplicationATOFINA Polypropylene PPH 5042 has been specially designed for extrusion-thermoforming, where it gives improved rigidity and impact resistanc.. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Melting Point | 165 °C | 329 °F | |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamOfin PPH307G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | Unpolymerized resin |
Cyclics CBT® 200 Thermoplastic Resin CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Melting Point | 165 - 170 °C | 329 - 338 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 165 °C | 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecoform® PO30 GR20 NL HS POM, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 526 N30 Polypropylene Homopolymer Improved rigidity, high durabilityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 °C | 329 °F | |
3M Dyneon™ THV 505ESDZ Fluoroplastic Granules Fluoroplastic THV is a flexible, fluoroplastic electrostatic dissipative compound composed of tetrafluoroethylene, hexafluoropropylene and vinylidene fluoride in the form of pellets.Information prov.. |
|||
Melting Point | 165 °C | 329 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROLEN PP GF 30 Polypropylene 30% glass fiber This material is a low density, easily machined plastic that has high impact resistance and dimensional stability. Applications include air filter housings, fan blades, and fittings with high loads... |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 552 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |