Indium Corp. Indalloy 91 Indium Solder Alloy

Category Metal , Nonferrous Metal , Indium Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 91 Indium Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Thermal Properties Metric English Comments
Melting Point 153 °C
307 °F
Solidus 153 °C
307 °F
Liquidus 153 °C
307 °F
Component Elements Properties Metric English Comments
Gallium, Ga 0.40 %
0.40 %
Indium, In 99.6 %
99.6 %