Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa @Thickness 3.17 mm |
8900 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 61.4 MPa @Thickness 3.17 mm |
8900 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 61.4 MPa @Thickness 3.17 mm |
8910 psi @Thickness 0.125 in |
|
KEP Kepital® F20 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Techmer ES Luriblend® POM CO TX10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%) and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 88 GF 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 61.4 MPa | 8910 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-10 Polycarbonate CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8910 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-20 Polycarbonate CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Styron EMERGEâ„¢ 4800-7 Polycarbonate EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Chase Plastics CP Pryme® A100HF ABS Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Chase Plastics CP Pryme® AC100 Acetal Copolymer Features: Alkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGeneral purposeGrease resistantLow moisture absorptionOil resistantResilientHigh rigiditySolv.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | |
Tra-Con Tra-Cast 3357 High Temperature Rigid Epoxy Casting System TRA-CAST 3357 is a smooth pouring, low viscosity casting resin system recommended for rigid, large mass potting, encapsulating, laminating, filament-winding and coil embedment applications where the.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Omni Plastics OmniTuff™ CPP GRC20 Copolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 61.4 MPa | 8900 psi | ASTM D638 |
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |