Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis RB206MO-06 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis RB206MO-06 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also features high heat distortion temperature. The additives are optimized to provide reduced tendency for mould plate-out. Applications: monolayer and multilayer bottles in the food or cosmetic industry (hot filling).Information provided by Borealis AG
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.600 g/cc
0.0181 - 0.0217 lb/in³
Density 0.902 g/cc
0.0326 lb/in³
ISO 1183
Melt Flow 1.9 g/10 min

@Load 1.90 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.19 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Elongation at Yield 12 %
12 %
50mm/min; ISO 527-2
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ISO 75-2
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 220 °C
374 - 428 °F
Die Temperature 180 - 220 °C
356 - 428 °F
Melt Temperature 180 - 220 °C
356 - 428 °F
Users viewing this material also viewed the following: