Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE D 5303 BLK Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH350LN Polypropylene, Homopolymer, High Flow, Nucleated, Lube, Injection Molding COPYLENE™ CH350LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM003 Polypropylene Impact Copolymer CM003 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformation provided .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM100LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding Medium impact, nucleated, antistat, injection molding. Applications: Household articles, pails, consumer products.Information provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss a.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR027 Polypropylene, Homopolymer, Mini-random, BOPP Mini-random homopolymer. Applications: BOPP film. Equivalent to Pro-fax® HL456JInformation provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified CR350CL-02 is a clarified, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release.Potential Applications: Injection moldi.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR350CS-01 Polypropylene Random Copolymer COPYLENE® CR350CS-01 is a clarified, reactor grade, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release for larger ar.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH050 Polypropylene, Homopolymer, Cast Film BOPP COPYLENE™ CH050 is a polypropylene controlled rheology homopolymer resin designed for Cast Film BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches, Pe.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH085 Polypropylene, Homopolymer, Cast Film COPYLENE™ CH085, a controlled rheology polypropylene homopolymer resin, is used in injection molding and cast film extrusion applications. Applications: Bags & Pouches, Stationery Film, Stretch Wra.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding COPYLENE™ CM350LN is a high melt flow, controlled rheology, medium impact polypropylene copolymer resin designed for injection molding applications requiring a good balance of stiffness, impact, re.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR030LN Polypropylene, Mini-Random Copolymer, Thermoforming COPYLENE™ CR030LN is a mini-random copolymer with a high performance nucleation system designed to yield high clarity thermoformed articles.Applications: ThermoformingInformation provided by Philli.. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
M. Holland Company CP710 Polypropylene Impact Copolymer AntistaticImpact copolymerGood flowGood impact resistanceNucleatedApplications: ClosuresHousehold goodsThin-walled parts |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
LyondellBasell Pro-faxâ„¢ SC973 Polypropylene Copolymer Description: Pro-faxâ„¢ Ultra SC973 fully formulated (antistatic, nucleated, slip modified), very high melt flow, impact polypropylene reactor copolymer resin is designed for injection molding ap.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/2-HP UV Polyolefin Catalyst CT/2-HP UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® and Polidiemme® ser.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications Product Description: Exact 0230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for both monolayer and multilayer co-extruded cast .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow Engage® 8402 Polyolefin Elastomer Description: Engage® 8402 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8402 pr.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem RP 344 RACO Random Polypropylene Copolymer RP 344 is a medium melt flow rate random copolymer. It is suitable for blown and cast film extrusion and features good processability, excellent optical properties, and outstanding sealability. Its .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem Symbios 3102 Polypropylene Terpolymer Braskem Symbios 3102 is a medium melt flow rate terpolymer with a heat seal temperature below 110ºC on its non-treated face. It is designed for use as a heat sealing layer for cast film coextrusion.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Bapolene® PP5052 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH034EV Polypropylene, Homopolymer, Fiber, Tape, UV COPYLENE™ CH034EV is a polypropylene homopolymer resin designed for fiber applications. Applications: Filament Yarn, Geotextile & agriculture. Equivalent to Pro-fax® HL348JInformation provided by .. |
|||
Density | 0.902 g/cc @Temperature 15.6 °C |
0.0326 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Mobil Almo 532 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer CM090L is a high impact copolymer with antistat and is specially designed to excel in injection molding processes for consumer products.Applications: Injection MoldingInformation provided by Phillip.. |