Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 250 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI 40 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified blend PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents, good dimensional stabilit.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | Condition G |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5G2K-096 Random Copolymer Polypropylene Features: Excellent clarity. Product does not contain animal derived components. Phthalate-freeApplications: Thermoforming, extrusion blow molding, injection blow molding, stretch blow molding, .. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-sanitary products, electrical partsInformation provided b.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B4020N1331 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B4020N1332 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0200RX Biocompatible LDPE A biocompatible Low Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0202AF Food Grade LDPE Low Density Polyethylene with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ISO 1133 |
Lucite International Diakon® TD525 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5M2Z-012 Polypropylene Random Copolymer Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos N01N-00 Polypropylene Impact Copolymer Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos N02J-00 Polypropylene Impact Copolymer This is a low melt flow rate, high impact copolymer polypropylene for sheet extrusion and thick wall injection molding applications. It offers a superior balance of stiffness and impact strength fo.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormed™ RB801CF Polypropylene Random Copolymer Bormed™ RB801CF is a random copolymer. Applications: Bormed™ RB801CF is intended for packaging for medical devices, pouches, and packaging for pharmaceutical products. Additives: Bormed™ RB801C.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont 20 Series DPE 20 Specialty Polyethylene Resin DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 3051 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3051 is homopolymer.ApplicationATOFINA Polypropylene PPH 3051 is intended for the extrusion of flat bioriented films for food packaging or high strength adhesive tapes. Inf.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow 6D20 Polypropylene Resin DOW 6D20 is intended for use in film and extrusion blow molding processes. It is especially suited for multilayered, barrier bottles.Information provided by DowDow Announced Sale of Global Polyprop.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg |
1.9 g/10 min @Load 4.76 lb |
|
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow 6D83K Polypropylene Resin DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem PB682 Blow Molding Low Density Polyethylene Blow molding; Injection blow molding; Medium resistance mechanical film; Expanded PE blankets.Information provided by Braskem. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® E 65 F Polypropylene Homopolymer Description: CAPILENE® E 65 F is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It exhibits good processability, easy film stretchabilit.. |
|||
Melt Flow | 1.9 g/10 min @Load 1.90 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.19 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRx™ PE3-0201A Antimicrobial LDPE Low Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc. |