Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Start Point: 205°C |
Kingfa FW-650 Flame Retardant ABS Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 4785 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 817 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walle.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BB108E Polypropylene compound for Steel Pipe Coating BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis BB125MO Polypropylene Copolymer BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | cylinder |
Borealis Borcoat™ BA213E Polypropylene for Steel Pipe Coating Borcoat™ BA213E is a polypropylene compound used as a component in thermal insulation coating systems. Applications: Borcoat™ BA213E is recommended as a polymer to make foam for thermal insulatio.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | cylinder |
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im.. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis RB607MO Polypropylene Random Copolymer RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion .. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Diamond Polymers ABS 3502ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Diamond Polymers ABS 4000HH-ELG Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Diamond Polymers ABS 7600B (ELG) Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Diamond Polymers ABS 9301 Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical KEYFLEX TO1088AV Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0Information provided by LG Chemical |