Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 180 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
PolyOne OnFlex™ HT 40A-3S2131 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
Melt Temperature 180 - 220 °C
356 - 428 °F
Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion
Information provided by Polykemi AB
Melt Temperature 180 - 220 °C
356 - 428 °F
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin
Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer.
Melt Temperature 180 - 220 °C
356 - 428 °F
Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced
Information provided by Polykemi AB
Melt Temperature 180 - 210 °C
356 - 410 °F
Lotte Chemical Titan TITANEX® LF0754 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF0754 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant agent. This product is used for blown film extrusion which offers outstanding toughness, extrudabilit..
Melt Temperature 180 - 200 °C
356 - 392 °F
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and ..
Melt Temperature 180 - 200 °C
356 - 392 °F
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® M25UV POM, UV Resistant  (Unverified Data**)
Celcon® M25UV is an acetal copolymer developed as a natural UV light stabilized low flow, high molecular weight grade. It has been formulated as a natural acetal that does not discolor, yet maintai..
Melt Temperature 180 - 246 °C
356 - 475 °F
Average value: 219 °C Grade Count:7
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Melt Temperature 180 - 220 °C
356 - 428 °F
Injection Molding
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 180 - 280 °C
356 - 536 °F
Molding
Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA)
Description: Avantra® 594E is a super high-impact polystyrene grade that delivers excellent processing efficiency along with toughness and high gloss in a wide variety of injection molding applic..
Melt Temperature 180 - 280 °C
356 - 536 °F
Molding
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren..
Melt Temperature 180 - 240 °C
356 - 464 °F
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin
HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag..
Melt Temperature 180 - 220 °C
356 - 428 °F
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin
HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci..
Melt Temperature 180 - 230 °C
356 - 446 °F
Injection Molding
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 180 - 230 °C
356 - 446 °F
Extrusion
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 180 - 230 °C
356 - 446 °F
Injection Molding
Stellarchem AB870EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 180 - 260 °C
356 - 500 °F
ISO 294
Styrolution PS 476L HIPS
Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl..
Melt Temperature 180 - 260 °C
356 - 500 °F
Supreme Petrochem SC 202LV General Purpose Polystyrene
CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products ..
Melt Temperature 180 - 260 °C
356 - 500 °F
Supreme Petrochem SC 203EL General Purpose Polystyrene
CharacteristicsMedium flow grade with good mechanical properties Improves productivity due to good balance of flow, heat and mold release propertiesProcessing Injection moldingApplicationsAudio cass..
Melt Temperature 180 - 220 °C
356 - 428 °F
Borealis BL0521 High Density Polyethylene
BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums ..
Melt Temperature 180 - 220 °C
356 - 428 °F
Borealis BL2571 High Density Polyethylene
BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers..
Melt Temperature 180 °C
356 °F
Extrusion
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Lumicene® mPE M 5220 is a high density polyethylene with outstanding organoleptic properties, stress-cracking resistance and processability.Lumicene® mPE M 5220 is especially suited for the produc..
Melt Temperature 180 - 240 °C
356 - 464 °F
RTP Company RTP 2999 X 125934 A NS Polyether-Block-Amide (PEBA / COPA); Barium Sulfate Filled
Melt Temperature 180 - 205 °C
356 - 401 °F
Covestro Desmopan® 9385 Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9362 POM, Impact Modified
Hostaform« acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform« S 9362 provides good impact strength while improving modulus and weld ..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® C 13021 XAP² ™ POM, Unfilled
POM copolymerInformation provided by Celanese
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9363 POM, Impact Modified
Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® MT12R01 POM, Medical Technology
Hostaform« MT12R01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12R01 is a low melt viscosity and improved ..
Melt Temperature 180 - 260 °C
356 - 500 °F
Average value: 215 °C Grade Count:49
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Copyright © lookpolymers.com All Rights Reserved