Mechanical Properties Metric English Comments
Tensile Modulus 1.15 GPa
167 ksi
Radici Radilon® S 40E (cond.) Nylon 6
PA6 high viscosity injection molding suitable also for extrusion.Information provided by Radici group.
Tensile Modulus 1.15 GPa
167 ksi
ISO 527
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Tensile Modulus 1.15 GPa
167 ksi
1 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-9514 is a 10% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9514 is dev..
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ISO 527-2
Borealis Bormed™ HE9621-PH HDPE for Healthcare Applications
Bormed HE9621-PH is a natural HD polyethylene with narrow molecular weight distribution, produced in low-pressure gas-phase process. This grade is designed for the injection molding of articles whe..
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ASTM D638
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Bormed RF825MO is a specially modified random copolymer polypropylene with high melt flow intended for use in medical and medical related articles. Bormed RF825MO is characterized by easy processab..
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ASTM D638
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications
Bormed RF830MO is a specialty modified random copolymer polypropylene with high melt flow intended for use in medical and medical related articles. Bormed RF830MO is characterized by easy processab..
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ISO 527-2
Borealis Daplen™ EE115AE TPO Compound
Daplen EE115AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115AE is a material with excellent impact /stiffness ratio. Thanks to its low ..
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ISO 527-2
Borealis Daplen™ EE115T TPO Compound
Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th..
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Borealis Daplen™ EH104AE Polypropylene TPO Compound
Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high..
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Borealis MG9621B Polyethylene
Applications: crates, and pailsInformation provided by Borealis AG
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Borealis MG9621S Polyethylene
MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Borealis RF926MO Polypropylene, Transparent Random Copolymer
RF926MO is a specially modified transparent polypropylene random copolymer with high melt flow. This grade is intended for injection stretch blow molding (ISBM). and is designed for high-speed injec..
Tensile Modulus 1.15 GPa
167 ksi
ISO 527-2
Total PPC 9712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de..
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ISO 527-2
Borealis Daplen™ EE015U TPO Compound
Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th..
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Borealis RB206MO Polypropylene Random Copolymer
RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also ..
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-3
Borealis RF365MO Polypropylene
Applications: closures, thin wall containers, and excellent transparency.Information provided by Borealis AG
Tensile Modulus 1.15 GPa
167 ksi
ISO 527-2
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact..
Tensile Modulus 1.15 GPa
167 ksi
ISO 527-2
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &..
Tensile Modulus 1.15 GPa
167 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ CNU 011 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications in which good surface finish and UV resistance is required. Availabilit..
Tensile Modulus 1.15 GPa
167 ksi
ISO527-2/1
ExxonMobil PP7085E1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica..
Tensile Modulus 1.15 GPa
167 ksi
ISO 527-2
Domo 2448L Polypropylene Copolymer
Information provided by Domo.
Tensile Modulus 1.15 GPa
167 ksi
ISO 527-2
Domo 2600M Polypropylene Copolymer
Information provided by Domo.
Tensile Modulus 1.15 GPa
167 ksi
ISO 527
Dow INSPIRE™ 112 Performance Polymer
INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow
Tensile Modulus 1.15 GPa
167 ksi
BASF Novolen® 2448 L Polypropylene
Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.15 GPa
167 ksi
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Tensile Modulus 1.15 GPa
167 ksi
BASF Novolen® 2660 M Polypropylene
UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.15 GPa
167 ksi
BASF Novolen® 3248 TC Polypropylene
Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.15 GPa
167 ksi
BASF Procom® D 1118 Polypropylene
Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Borealis RB206MO-06 Polypropylene Random Copolymer
RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als..