Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 356 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion
Information provided by Polykemi AB
Melt Temperature 180 - 220 °C
356 - 428 °F
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Melt Temperature 180 - 220 °C
356 - 428 °F
Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
Melt Temperature 180 - 200 °C
356 - 392 °F
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin  (discontinued **)
LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® GB10 POM, 10% Glass Reinforced  (Unverified Data**)
Celcon® GB10 is a 10% glass bead filled grade for low shrinkage and warp resistance in large, flat, and thin walled parts.10% glass bead, low warpage, has been replaced by Hostaform® C 9021 GV3/10..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® LW25-S2 POM, Tribological  (Unverified Data**)
Celcon® LW25-S2 acetal copolymer is a low flow, improved toughness product formulated with a low level of silicone to reduce friction and improved wear resistance.Low wear/friction, silicone, low s..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® C 9021 XAP² ™ POM  (Unverified Data**)
POM copolymerLow EmissionInformation provided by Celanese
Melt Temperature 180 - 230 °C
356 - 446 °F
Celanese Hostaform® MT8F02 POM, Medical Technology  (Unverified Data**)
Hostaform® acetal copolymer grade MT8F02 is a special grade developed for medical industry applications containing low residual monomers. Hostaform® MT8F02 is a standard flow high level polytetra..
Melt Temperature 180 - 200 °C
356 - 392 °F
Extrusion Blow Molding
LG Chemical LUTENE-H BE0400 HDPE
Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con..
Melt Temperature 180 - 280 °C
356 - 536 °F
Molding
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene
Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic..
Melt Temperature 180 - 280 °C
356 - 536 °F
Molding
Ineos Styrenics Polystyrene 148G (NAFTA)
High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance.Information prov..
Melt Temperature 180 - 230 °C
356 - 446 °F
Injection Molding
Stellarchem AB835EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 180 - 280 °C
356 - 536 °F
ISO 294
Styrolution PS 124 N/L GPPS
Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor..
Melt Temperature 180 - 280 °C
356 - 536 °F
ISO 294
Styrolution PS 153F GPPS
Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica..
Melt Temperature 180 - 260 °C
356 - 500 °F
ISO 294
Styrolution PS 454N HIPS
Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss..
Melt Temperature 180 - 260 °C
356 - 500 °F
Supreme Petrochem SH 2157 High Impact Polystyrene
Characteristics Excellent ESCR properties Good formability Processing ExtrusionApplications Refrigerator door and cabinet liners Dairy containers Ice cream cups, plates and bowlsMaterial Status: ..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® GC90UV POM, 10% UV Resistant
Celcon« acetal copolymer grade GC90UV is a specialty grade combining glass coupling for improved strength and stiffness and UV stabilization for improved performance in exposure to artificial light..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® M90-45H POM, UV Resistant
Celcon« M90-45H is an acetal copolymer which has been stabilized to give protection against property and color degradation in interior applications where UV exposure is anticipated.Information prov..
Melt Temperature 180 - 195 °C
356 - 383 °F
Celanese Hostaform® LX90Z POM, UV Resistant
Hostaform« LX90Z specialty metallic appearance grades are an integrally colored nominal 9 melt flow rate based acetal copolymer material stabilized for use where ultraviolet radiation exposure is t..
Melt Temperature 180 - 190 °C
356 - 374 °F
Celanese Hostaform® M90XAP® POM, Unfilled
Hostaform« acetal copolymer grade M90 XAP« is a low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the interior automo..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® MT8F02 POM, Medical Technology
Hostaform« acetal copolymer grade MT8F02 is a special grade developed for medical industry applications containing low residual monomers. Hostaform« MT8F02 is a standard flow high level polytetra..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® TF-10XAP® POM, Impact Modified
Hostaform« acetal copolymer TF-10 XAP« is low emission, improved flow, impact modified grade providing optimum performance in general purpose injection molding primarily for the interior automot..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9362 XAP2 ™ POM, Impact Modified
Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® EC140CF10 POM, 10% Specialty
Hostaform« acetal copolymer grade EC140CF10 is a 10% carbon fiber reinforced grade for increase strength, stiffness and electrical conductivity.Information provided by Celanese
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Hostaform® SlideX™ C0304 XAP² ™ POM, Tribological
POM copolymerInformation provided by Celanese
Melt Temperature 180 - 204 °C
356 - 399 °F
Celanese Riteflex® 640 Thermoplastic Polyester Elastomer (TPE)
Information provided by Celanese Corporation.
Melt Temperature 180 - 220 °C
356 - 428 °F
NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu..
Melt Temperature 180 - 220 °C
356 - 428 °F
Polykemi AB POLYfill PPH DNH15025 GF10 Polypropylene Homopolymer, Flame Retardant, Halogen Free, Glass Fibre-Reinforced
Information provided by Polykemi AB
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® LW90-S2 POM, Tribological  (Unverified Data**)
Celcon® LW90-S2 is a preblended low wear formulation of M90 base polymer containing 2% silicone. This standard low friction, low wear product performs well in many applications including those inv..
Melt Temperature 180 - 200 °C
356 - 392 °F
Celanese Celcon® WR90Z POM, UV Resistant  (Unverified Data**)
Celcon® WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of ..
Copyright © lookpolymers.com All Rights Reserved