Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 170 - 220 °C | 338 - 428 °F | |
Plastcom PLASTALEN® EQ 18 N Polyethylene Impact modified PE for extrusion. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Melt Temperature | 171 - 220 °C | 340 - 428 °F | Average value: 190 °C Grade Count:8 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | |
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Melt Temperature | 160 - 220 °C | 320 - 428 °F | |
Lucobit Lucofin® 1454 Polyolefin TPO Granules, Green Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Melt Temperature | 160 - 220 °C | 320 - 428 °F | |
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Melt Temperature | 160 - 220 °C | 320 - 428 °F | |
Lucobit Lucofin® 1455MB Polyolefin TPO Granules, Black Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection molding |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6017 Polypropylene Random Copolymer RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | |
E-Polymers SEPAZ® LH30 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 182 - 220 °C | 360 - 428 °F | Average value: 204 °C Grade Count:14 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |