Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol R019MZ Polypropylene REPOL Polypropylene R019MZ is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
BP Amoco Acctuf® 3119HS Ultra High Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High stiffness, Low Temperature impactComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills 43S2A Polypropylene Random Copolymer Features: Good clarity.Applications: Film extrusion and blow moldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5L2K-055 Polypropylene Random Copolymer Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow moldin.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-sanitary products, electrical partsInformation provided b.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B4020N1331 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B4020N1332 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0202AF Food Grade LDPE Low Density Polyethylene with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ISO 1133 |
Lucite International Diakon® TD525 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos N01N-00 Polypropylene Impact Copolymer Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon Tabond 2006 Adhesive Resin Tabond 2006 is a chemically modified thermoplastic polyolefin with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated g.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex ELEXAR® EL 8712 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont 20 Series DPE 20 Specialty Polyethylene Resin DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow 6D20 Polypropylene Resin DOW 6D20 is intended for use in film and extrusion blow molding processes. It is especially suited for multilayered, barrier bottles.Information provided by DowDow Announced Sale of Global Polyprop.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg |
1.9 g/10 min @Load 4.76 lb |
|
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Arkema Group Kynar® FLEX 2750 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne.. |
|||
Melt Flow | 1.9 g/10 min @Load 1.90 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.19 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
M. Holland Company MAGMA® LM213-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |