Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.510 - 0.600 g/cc | 0.0184 - 0.0217 lb/in³ | PVCH/QCD/3516 |
Reliance Industries 67-01 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusion.Can be used:rigid injection. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Magyar Aluminum ALO-P90-06 Alumina Alumina for Polishing |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Magyar Aluminum ALO-P95-06 Alumina Alumina for Polishing |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Magyar Aluminum ALO-P95-08 Alumina Alumina for Polishing |
|||
Bulk Density | 0.520 - 0.600 g/cc | 0.0188 - 0.0217 lb/in³ | ASTM D1895 |
LG Chemical LS080S PVC General Description: LS080S, homopolymer made by suspension polymerization, can be applied to hard or semi-hard products.Main Applications: Hard sheets, films, fittings, injection molded products, b.. |
|||
Bulk Density | 0.520 - 0.600 g/cc | 0.0188 - 0.0217 lb/in³ | ASTM D1895 |
LG Chemical LS100E PVC General Description: LS100E, homopolymer by mass polymerization, can be applied to various applications, such as semi rigid and rigid products.Main Applications: Pipe, profiles, sashCAS No: 9002-86-.. |
|||
Bulk Density | 0.450 - 0.600 g/cc | 0.0163 - 0.0217 lb/in³ | |
Gromax EP-5016M Unplasticized Vinyl Acetate homopolymer Product Description: EP-5016M is a water redispersible vinyl acetate homopolymer powder that is readily dispersible in water and forms stable emulsion. This redispersible powder is especially recomm.. |
|||
Bulk Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Solvay Chemicals KaCeFlux Potassium Fluoroaluminate Standard flux for brazing aluminum.HS No.: 3810100000 /CAS-No.: 60304-36-1 and 14484-69-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electri.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HLC-40B PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis Borcell™ HE1346 High Density Polyethylene Borcell™ HE1346 is a fully formulated compound for chemical foamed telesingles. Borcell™ HE1346 is a high-density polyethylene compound containing chemical blowing agent.
Applications Borcell™ HE.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis LE4244R Polyethylene Insulation Compound, Crosslinkable LE4244R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. This product is only available in certain periods. Applications: LE4244R is intended for in.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis SuperCOPO™ LH4201R Polyethylene Insulation Compound, Crosslinkable SuperCOPO™ LH4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LH4201R is intended for insulation of XLPE power cabl.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Addcomp ADD-MAX® 104 Efficiency masterbatch, LDPE based Fields of application: Masterbatch for improvement of production efficiency and product quality.Examples: PP, HDPE and LLDPE cast and blown films, pipes, tubes, wire and cables, blow molding and gen.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Addcomp ADD-VANCE® UV 442 PP based anti-UV masterbatch Fields of application: Foils, films, fibres, extruded and injection moulded articles made from PE and PP compatible resins, like PP, PP/EDPM, PP/PE/EDPM blends (TPOs).Examples: Automotive bumpers, a.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF Hydroxypivalic Acid Neopentylglycolester (HPN Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester (HPN) is a colorless, odorless solid.Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopentyl hydroxypiva.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF Hydroxypivalic Acid Neopentylglycolester Molten (HPN) Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester Molten (HPN) is a colorless, odorless molten solid. Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopen.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF 2-Methyl Imidazole Flake Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazoleApplications: Intermediate used in Pharmac.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF 2-Methyl Imidazole Pure Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazolApplications: Intermediate used in Pharmac.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Addcomp ADD-VANCE® SA 390 Slip Masterbatch, 30% active ingredients in polypropylene Fields of application: Imparts processing improvements and modified surface characteristics for extruded and injection molded articles made from polyolefins, polyester, and other polymersExamples: F.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size) Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE shou.. |