Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Network Polymers NPP 25-1011B Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH120LN Polypropylene, Homopolymer, Injection Molding, Antistat/Lube COPYLENE™ CH120LN is designed for general purpose injection molding applications with anti-static and nucleation. Applications: Food Containers, Housewares, Closures.Information provided by Phillip.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH180V Polypropylene, Homopolymer, BCF, UV, Gas Fading COPYLENE™ CH180V is a high melt flow polypropylene homopolymer resin designed for fiber spinning applications that require resistance to gas fading. Applications: Filament Yarn, Geotextile & agricu.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH200L Polypropylene, Homopolymer, CR, Antistat, Injection Molding COPYLENE™ CH200L is designed for general purpose injection molding applications with anti-static and controlled rheology. Applications: Food Containers, Housewares, Closures.Information provided by.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH350V Polypropylene, Homopolymer, Extrusion Coating, Spunbound, Gas Fade & UV Resistant COPYLENE™ CH350V is a very high melt flow polypropylene homopolymer resin designed for fiber spinning. Applications: Food Packaging Film, Heavy Duty Packaging, Absorption & Filtration, Filament Yar.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming COPYLENE™ CM040LN is an impact copolymer specially designed for excellent processing in thermoforming applications and is formulated with antistat and nucleation. Applications: Thermoforming, Injec.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation pro.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH050 Polypropylene, Homopolymer, Cast Film BOPP COPYLENE™ CH050 is a polypropylene controlled rheology homopolymer resin designed for Cast Film BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches, Pe.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer COPYLENE™ CM015 is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications: Injection M.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM200LN-02 Polypropylene Impact Copolymer COPYLENE™ CM200LN-02 is specially designed for injection molding applications where an excellent balance of stiffness/impact and good cycle times are required.Applications: Injection molding applic.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding COPYLENE™ CM350LN is a high melt flow, controlled rheology, medium impact polypropylene copolymer resin designed for injection molding applications requiring a good balance of stiffness, impact, re.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR030LN Polypropylene, Mini-Random Copolymer, Thermoforming COPYLENE™ CR030LN is a mini-random copolymer with a high performance nucleation system designed to yield high clarity thermoformed articles.Applications: ThermoformingInformation provided by Philli.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
LyondellBasell Pro-faxâ„¢ SC204 Polypropylene Copolymer Description: Pro-faxâ„¢ SC204 polypropylene copolymer resin is designed for thermoforming and sheet extrusion applications. It is nucleated and features antistatic properties. Pro-faxâ„¢ SC20.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
LyondellBasell Pro-faxâ„¢ SC973 Polypropylene Copolymer Description: Pro-faxâ„¢ Ultra SC973 fully formulated (antistatic, nucleated, slip modified), very high melt flow, impact polypropylene reactor copolymer resin is designed for injection molding ap.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
LyondellBasell Hifaxâ„¢ CA260GC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA260GC White fractional melt flow, 40 MPa flexural modulus, UV-stabilized, precolored thermoplastic elastomeric olefin (TEO) resin has an excellent balance of flexibility,.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications Bormed HF855MO is a high modulus polypropylene homopolymer and is especially developed within the proprietary Borstar technology. Bormed HF855MO combines an unique balance of properties for high sp.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis HH450MO Polypropylene HH450MO is a polypropylene homopolymer intended for injection molding. This grade is especially suitable for high-speed injection molding of articles demanding easy flow. This polymer is a CR (cont.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications Product Description: Exact 0230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for both monolayer and multilayer co-extruded cast .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Dow AFFINITY™ SM 1300 Polyolefin Plastomer AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow Engage® 8402 Polyolefin Elastomer Description: Engage® 8402 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8402 pr.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem PRB 0131 RACO Random Polypropylene Copolymer PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low h.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem Prisma 2910 RACO Random Polypropylene Copolymer Prisma 2910 is a high melt flow rate random copolymer designed for injection molding applications. This product offers high impact strength at low temperatures and excellent processability. Its appl.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem Symbios 3102 Polypropylene Terpolymer Braskem Symbios 3102 is a medium melt flow rate terpolymer with a heat seal temperature below 110ºC on its non-treated face. It is designed for use as a heat sealing layer for cast film coextrusion.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH034W Polypropylene, Homopolymer, Slit Film, LWCO COPYLENE™ CH034W is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Housewares, Raffia/tapes/strapping. Equivalent to P.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH200LN-02 Polypropylene, Homopolymer, Rx grade, Nucleated, Lube, Injection Molding COPYLENE™ CH200LN-02 is a polypropylene homopolymer resin nucleated for faster crystallization with antistatic properties and designed for injection molding applications. Applications: Caps & Closu.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer CM090L is a high impact copolymer with antistat and is specially designed to excel in injection molding processes for consumer products.Applications: Injection MoldingInformation provided by Phillip.. |