Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C @Thickness 3.20 mm |
187 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C @Thickness 3.20 mm |
187 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 - 202 °C | 187 - 396 °F | Average value: 122 °C Grade Count:14 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CH085 Polypropylene, Homopolymer, Cast Film COPYLENE™ CH085, a controlled rheology polypropylene homopolymer resin, is used in injection molding and cast film extrusion applications. Applications: Bags & Pouches, Stationery Film, Stretch Wra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | |
Eastman Tenite 105-33 Cellulose Acetate
(discontinued **) 33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | |
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM D648 |
Flint Hills P9H8M-015 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Ineos H03G-04 Polypropylene Homopolymer This is a polypropylene homopolymer for biaxially oriented polypropylene (BOPP) film and blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM D648 |
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | 80*10*4mm, Cut; ISO 75-1&2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C @Thickness 3.20 mm |
187 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C @Thickness 3.20 mm |
187 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp CF006 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF006 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ISO 75-2 |
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ISO 75 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM D648 |
Total PPC 5724 Polypropylene, Extra High Impact Copolymer ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ISO 75-2 |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM D648 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ISO 75-2/B |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ISO 75-2/B |
ExxonMobil PP5032E3 Polypropylene Copolymer Product Description: A polypropylene homopolymer type designed for production of monofilaments, tapes for the textile industry, geo textiles, fibrillated tapes for ropes and twines in the packaging.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437W20L1 Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM-D648 |
Braskem RP 344 RACO Random Polypropylene Copolymer RP 344 is a medium melt flow rate random copolymer. It is suitable for blown and cast film extrusion and features good processability, excellent optical properties, and outstanding sealability. Its .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM D-648 |
Bapolan® 6055 Polystyrene, Injection Molding Bapolan PS6055 is a crystal polystyrene resin designed for injection molding applications requiring fast cycle times and superior optical properties. It complies with US FDA21 CFR177.1640 and 94HB .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | ASTM D648 |
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy Dimensional StabilityInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | |
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.0 °C | 187 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 425 High Impact Polystyrene
(discontinued **) STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper.. |