Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
24 hr in water at 20°C; ASTM D570
Water Absorption at Saturation 0.60 %
0.60 %
20°C and 65% RH; ASTM D570
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength at Break 52.0 MPa
7540 psi
ASTM D638
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
Elongation at Yield 18 %
18 %
ASTM D638
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256-A
0.500 J/cm

@Temperature -40.0 °C
0.937 ft-lb/in

@Temperature -40.0 °F
ASTM D256-A
Izod Impact, Unnotched NB
NB
ASTM D256-A
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D256-A
Thermal Properties Metric English Comments
Heat of Fusion 54.0 J/g
23.2 BTU/lb
ASTM D3417
CTE, linear 160 µm/m-°C

@Temperature -40.0 - 140 °C
88.9 µin/in-°F

@Temperature -40.0 - 284 °F
ASTM D696
Melting Point 172 °C
342 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Vicat Softening Point 165 °C
329 °F
under 1 daN; ASTM D1525
Electrical Properties Metric English Comments
Surface Resistance 4.00e+13 ohm

@Temperature 20.0 °C
4.00e+13 ohm

@Temperature 68.0 °F
65% RH; ASTM D257