Material Notes:
EXCEREXâ„¢ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREXâ„¢ gains in a number of ares simultaneously, including faster processing speeds, lower resin temperatures, reduced scorching, and reduced changeover times.Information provided by Mitsui Chemicals
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
Molecular Weight 4600 g/mol
4600 g/mol
Thermal Properties Metric English Comments
Melting Point 90.0 °C
194 °F
Softening Point 98.0 °C
208 °F