Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 160 µm/m-°C @Temperature 23.0 - 100 °C |
88.9 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murflor® Polytetrafluoroethylene Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with.. |
|||
CTE, linear | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359 |
Polikim Polypropylene Polypropylene is an olefin class plastic with low density. It has good chemical and electrical properties and is rigid. Its use under 0°C is not recommended as its mechanical properties weaken. Nor.. |
|||
CTE, linear | 160 µm/m-°C @Temperature -40.0 - 149 °C |
89.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
|
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
CTE, linear | 160 µm/m-°C | 88.9 µin/in-°F | ASTM D696 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 160 µm/m-°C | 88.9 µin/in-°F | Alpha 2 |
Lord Adhesives Thermosetâ„¢ MD-150 Conductive Adhesive LORD Thermosetâ„¢ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing app.. |
|||
CTE, linear | 160 - 190 µm/m-°C | 88.9 - 106 µin/in-°F | DIN 52328 |
Isoflon PUR Polyurethane Very high wear resistanceHighly resilientInformation provided by Isoflon. |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo Pelprene™ P-70B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
|
Total HP 401 MDPE, pipe, cable, sheet FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit.. |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
|
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
|
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
CTE, linear | 160 µm/m-°C @Temperature -20.0 - 32.0 °C |
88.9 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
CTE, linear | 160 µm/m-°C @Temperature -20.0 - 32.0 °C |
88.9 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
CTE, linear | 160 µm/m-°C | 88.9 µin/in-°F | |
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
CTE, linear | 160 µm/m-°C @Temperature -40.0 - 140 °C |
88.9 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
CTE, linear | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
|
Total Lacqtene® 2001 TBK 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and .. |
|||
CTE, linear | 160 µm/m-°C @Temperature -20.0 - 32.0 °C |
88.9 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
CTE, linear | 160 µm/m-°C | 88.9 µin/in-°F | ASTM D696 |
Manifattura Cattaneo PP-s Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |