Shin-Etsu Silicones Primer 4 Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones Primer 4 Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primer 4 is a primer designed for bonding platinum or peroxide cure type silicone products to metals including aluminum and various plastics.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.780 g/cc
0.780 g/cc