Electrical Properties Metric English Comments
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
ASTM D257
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
ASTM D257
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX102R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
Surface Resistance 4.00e+13 ohm

@Temperature 20.0 °C
4.00e+13 ohm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay..
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..