Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber/Solid Lube Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Nylatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”. The elimination of stick-slip, mostly associated with chatter or squeaking, provides an amount of motion control for high-precision applications. High mechanical strength, stiffness, hardness and toughness Good fatigue resistance High mechanical damping ability Good sliding properties Excellent wear resistance Good electrical insulating properties Good resistance to high energy radiation (gamma- and X-rays) Good machinability
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50% RH
Water Absorption at Saturation 6.3 %
6.3 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 59
59
ISO 2039-2
Hardness, Shore D 73
73
Ball Indentation Hardness 120 MPa
17400 psi
ISO 2039-1
Tensile Strength 60.0 MPa
8700 psi
at Yield; ISO 527-1/-2
Elongation at Break 15 %
15 %
ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-1/-2
Tensile Modulus 2.75 GPa
399 ksi
ISO 527-1/-2
Compressive Strength 26.0 MPa

@Strain 1 %
3770 psi

@Strain 1 %
ISO 604
48.0 MPa

@Strain 2 %
6960 psi

@Strain 2 %
ISO 604
69.0 MPa

@Strain 5 %
10000 psi

@Strain 5 %
ISO 604
K Factor (ISO) 2.5 µm/km
2.5 µm/km
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.12 - 0.18
0.12 - 0.18
Limiting Pressure Velocity 0.300 MPa-m/sec
8570 psi-ft/min
at 1 m/s unlubricated
0.480 MPa-m/sec
13700 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 23.0 - 100 °C
55.6 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Melting Point 215 °C
419 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous; 20,000 h
105 °C
221 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index <= 20 %
<= 20 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: