Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C

@Temperature 23.0 - 100 °C
88.9 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murflor® Polytetrafluoroethylene
Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with..
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
ISO 11359
Polikim Polypropylene
Polypropylene is an olefin class plastic with low density. It has good chemical and electrical properties and is rigid. Its use under 0°C is not recommended as its mechanical properties weaken. Nor..
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Humiseal 1C49 Silicone Conformal Coating
Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605..
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
ASTM D696
Manifattura Cattaneo PE HD Polyethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
Alpha 2
Lord Adhesives Thermosetâ„¢ MD-150 Conductive Adhesive
LORD Thermosetâ„¢ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing app..
CTE, linear 160 - 190 µm/m-°C
88.9 - 106 µin/in-°F
DIN 52328
Isoflon PUR Polyurethane
Very high wear resistanceHighly resilientInformation provided by Isoflon.
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo Pelprene™ P-70B Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Total HP 401 MDPE, pipe, cable, sheet
FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit..
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
CTE, linear 160 µm/m-°C

@Temperature -20.0 - 32.0 °C
88.9 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc
Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
CTE, linear 160 µm/m-°C

@Temperature -20.0 - 32.0 °C
88.9 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc
Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam
EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds
CTE, linear 160 µm/m-°C

@Temperature -40.0 - 140 °C
88.9 µin/in-°F

@Temperature -40.0 - 284 °F
ASTM D696
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA)
Information provided by Arkema Group
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Total Lacqtene® 2001 TBK 46 HDPE pipe  (discontinued **)
LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and ..
CTE, linear 160 µm/m-°C

@Temperature -20.0 - 32.0 °C
88.9 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc  (discontinued **)
Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
ASTM D696
Manifattura Cattaneo PP-s Polypropylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.