Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | ASTM D257 |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | ASTM D257 |
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Surface Resistance | 4.00e+13 ohm @Temperature 20.0 °C |
4.00e+13 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | |
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Surface Resistance | 4.00e+13 ohm | 4.00e+13 ohm | |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |