Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 165 °C | 329 °F | ISO 306 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/h 50N; ISO 306 |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Vicat Softening Point | 165 - 220 °C | 329 - 428 °F | Average value: 208 °C Grade Count:18 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Vicat Softening Point | 165 °C @Load 5.10 kg |
329 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/h 50N; ISO 306 |
Lanxess Pocan® KU 2-7317 000000 PBT, 17% Glass Fiber PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warp, impact modified |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/h 50N; ISO 306 |
Lanxess Pocan® S 7926 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |
|||
Vicat Softening Point | 165 °C | 329 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-8030 Polyacetal-copolymer, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latigray 82-03 CW/95 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latigray 82-04 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 165 °C | 329 °F | VST/A/50; ISO 306 |
Styrolution Terblend® N NM-13 ABS+PA (Conditioned) Description: Terblend® N NM-13 is ABS/PA blend combining excellent impact strength at low temperatures with easy processability and good surface appearance.Information provided by STYROLUTION, wh.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Vicat Softening Point | 165 °C | 329 °F | A (10N); ISO 306 |
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance.. |
|||
Vicat Softening Point | 165 °C | 329 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
Vicat Softening Point | 165 °C | 329 °F | |
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |
|||
Vicat Softening Point | 165 °C | 329 °F | A (10N); ISO 306 |
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL FR9310 PPE (Europe-Africa-Middle East) Noryl*FR9310 is a polyphenylene ether resin concentrate with nonhalogenated Flame retardant with Vicat of 165 deg C. Intended for use as an additive or a building block in a variety of thermoplasti.. |
|||
Vicat Softening Point | 165 - 210 °C | 329 - 410 °F | Average value: 183 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C | 329 °F | B |
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-05 D040 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |