Material Notes:
40% glass reinforced, excellent dimensional stability and low water absorption. Also available as: 990LS-40G, same with heat stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 169 MPa
24500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 219 °C
426 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
424 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648