Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier |
Silicone Foam |
Bisco®
|
Rogers Corporation Bisco® EC-2130 Conductive Silicone |
Silicone |
Bisco®
|
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-1200 Solid Silicone Rubber |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-1500 Solid Silicone Rubber |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-200 Solid Silicone Rubber |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-6000 Solid Silicone Rubber |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ RF-120 Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Poron® 4701-15 Urethane Foam, Soft Seal |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Handheld Urethane Foam, Handheld Grade, PET Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron® Shock Seal™
|
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade |
Thermoset Polyurethane Foam, Unreinforced |
Poron® Shock Seal™
|
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade |
Thermoset Polyurethane Foam, Unreinforced |
Poron® Shock Seal™
|
Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade |
Thermoset Polyurethane Foam, Unreinforced |
Poron® Shock Seal™
|
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron® Shock Seal™
|
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron® ThinStik ShockSeal™
|
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron® ThinStik Soft Seal
|
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron® ThinStik Soft Seal
|
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron® ThinStik™
|
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam |
Thermoset Polyurethane Foam, Unreinforced |
Poron® ThinStik™
|
Rogers Corporation R/bak® SF Supported Firm Cushion Mounting Material |
Thermoset Polyurethane Foam, Unreinforced |
|
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft |
Thermoset Polyurethane Foam, Unreinforced |
|
Rogers Corporation R/bak® U Unsupported Cushion Mounting Material |
Thermoset Polyurethane Foam, Unreinforced |
|
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive |
Thermoset Polyurethane Foam, Unreinforced |
|
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO4450B Prepreg |
Thermoset |
|
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate |
Thermoset |
|
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate |
Thermoset |
|
Rogers Corporation RO4535 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate |
Thermoset |
|
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance |
Thermoset |
|
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RT/duroid® 6002 High Frequency Laminate |
Polymer |
|
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RT/duroid® 6202 High Frequency Laminate |
Polymer |
|
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate |
Polymer |
|
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material |
Thermoplastic |
Syron™
|
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material |
Thermoplastic |
Syron™
|
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material |
Polymer |
Theta®
|
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite |
Thermoset |
TMM®
|
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite |
Thermoset |
TMM®
|
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite |
Thermoset |
TMM®
|
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite |
Thermoset |
TMM®
|
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite |
Thermoset |
TMM®
|
Rogers Corporation Ultralam® 3850 Liquid Crystalline Polymer Circuit Material |
Polymer |
Ultralam®
|
Rogers Corporation Ultralam® 3908 Liquid Crystalline Polymer Circuit Material |
Polymer |
Ultralam®
|
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material |
Thermoplastic |
XT/duroid™
|
Rogers Corporation XT/duroid™ 8100 0.002" Woven Glass Reinforced Thermoplastic Circuit Material |
Thermoplastic |
XT/duroid™
|
Rogers Corporation XT/duroid™ 8100 0.004" Woven Glass Reinforced Thermoplastic Circuit Material |
Thermoplastic |
XT/duroid™
|
Rogers Corporation Bisco® MF1 6535 - 35 Silicone, High Performance Foam, Indentation Force Material |
Silicone Foam |
Bisco®
|
Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material |
Silicone Foam |
Bisco®
|
Rogers Corporation Bisco® MF1 9575 - 75 Silicone, High Performance Foam, Indentation Force Material |
Silicone Foam |
Bisco®
|
Rogers Corporation Bisco™ FPC Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam |
Rubber or Thermoset Elastomer (TSE) |
Bisco™
|
Rogers Corporation LoPro™ RO4730 Antenna Grade Non-PTFE Laminate |
Thermoset |
LoPro™
|
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced |
Thermoset Polyurethane Foam, Unreinforced |
Poron®
|
Rogers Corporation RO3035 Ceramic-Filled PTFE Composite, High Frequency Circuit Material |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO3730 Antenna Grade Laminate |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
|
Rogers Corporation RO4450F Prepreg |
Thermoset |
|
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film |
Fluoropolymer |
|
Rogers Corporation Bisco® A2 R 1.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier |
Silicone, Molded, Glass Fiber Filled |
Bisco®
|