Rogers Corporation Bisco™ HT-6000 Solid Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Rogers Corporation
Trade Name Bisco™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation Bisco™ HT-6000 Solid Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High purity silicone rubber, available extra thin in "film-like" sheet, down to 0.01" (0.25 mm) thickness. Applications: "Invisible" gaskets for enhancing cosmetic value, Flexible laboratory fixture covers, Transparent membranes on lab equipment and specimens, Airflow diaphragms on respirators and ventilators.General BISCO™ silicone information: BISCO™ Cellular Silicones are used as sealing cushioning, vibration isolation, insulation, and thermal management gaskets. Their resistance to environmental extremes, mechanical resilience, and safety features lead to their use in transportation equipment, communications and electrical enclosures, electronic products and components, industrial machinery, and appliances.Data provided by Rogers Corporation.
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified