Material Notes:
PORON® 4701-15 Improved Soft Seal SeriesEnhanced Surface Toughness, Reliable Materials for Thinner DesignsIncreased Surface Toughness, Improved YieldsExcellent Compressibility and ConformabilityLong Term Protection and SealingColor - Soft Seal GrayInformation provided by Rogers Corporation.
Physical Properties Metric English Comments
Density 0.104 g/cc
0.00376 lb/in³
ASTM D3574-95 Test A
1.395 g/cc
0.05040 lb/in³
supporting material; ASTM D1505
Thickness 533 - 991 microns
21.0 - 39.0 mil
Range of Thicknesses Available
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
15000 psi
F5, supporting material; ASTM D882
Elongation at Break 150 %
150 %
supporting material; ASTM D882
Tensile Modulus 3.45 GPa
500 ksi
MD, supporting material; ASTM D882
Compressive Yield Strength 0.00200 - 0.00462 MPa

@Strain 25.0 %
0.290 - 0.670 psi

@Strain 25.0 %
0.2"/min. strain rate, varies with thickness
Coefficient of Friction, Dynamic 0.40
0.40
A/B, supporting material; ASTM D1894
Compression Set <= 10 %

@Temperature 70.0 °C
<= 10 %

@Temperature 158 °F
ASTM D3574-95 Test D
Film Tensile Strength at Break, MD 207 MPa
30000 psi
supporting material; ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD 1.2 %

@Temperature 150 °C,
Time 2340 sec
1.2 %

@Temperature 302 °F,
Time 0.650 hour
supporting material
Shrinkage, TD 0.00 %

@Temperature 150 °C,
Time 2340 sec
0.00 %

@Temperature 302 °F,
Time 0.650 hour
supporting material