Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Rogers Corporation
Trade Name Poron® Shock Seal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thickness: 0.062"- 0.188"Color: BlackInformation provided by Rogers Corporation.
Physical Properties Metric English Comments
Density 0.320 g/cc
0.0116 lb/in³
ASTM D3574-95 Test A
Water Absorption 10 %

@Time 7200 sec
10 %

@Time 2.00 hour
Immersion; ASTM D570
Thickness 1570 - 4780 microns
62.0 - 188 mil
Range of Thicknesses Available
Mechanical Properties Metric English Comments
Tensile Strength >= 0.689 MPa
>= 100 psi
ASTM D3574-75 Test E
Elongation at Break >= 145 %
>= 145 %
ASTM D3574-75 Test E
Compressive Yield Strength 0.0276 - 0.110 MPa

@Strain 25.0 %
4.00 - 16.0 psi

@Strain 25.0 %
0.2"/min. strain rate
Tear Strength >= 1.80 kN/m
>= 10.3 pli
ASTM D642-91 Die C
Compression Set <= 5.0 %

@Temperature 23.0 °C
<= 5.0 %

@Temperature 73.4 °F
ASTM D3574-95 Test D
<= 10 %

@Temperature 70.0 °C
<= 10 %

@Temperature 158 °F
ASTM D3574-95 Test D
Descriptive Properties Value Comments
Flammability Test pass
MVSS 302; 0.062 in.