Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Rogers Corporation Bisco™ HT-1200 Solid Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Rogers Corporation
Trade Name Bisco™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation Bisco™ HT-1200 Solid Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specification grade solid silicone rubber available in durometers from 40 to 70 Shore A.Applications: General industrial gaskets for high temperatures and pressures, Gaskets on appliance motors and burners, Airflow diaphragms on respirators and ventilators, Automotive underhood gaskets.General BISCO™ silicone information: BISCO™ Cellular Silicones are used as sealing cushioning, vibration isolation, insulation, and thermal management gaskets. Their resistance to environmental extremes, mechanical resilience, and safety features lead to their use in transportation equipment, communications and electrical enclosures, electronic products and components, industrial machinery, and appliances.Data provided by Rogers Corporation.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved