Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 4760 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.120 - 1000 J/cm²
0.571 - 4760 ft-lb/in²
Average value: 1.40 J/cm² Grade Count:83
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Charpy Impact, Notched 0.300 - 1000 J/cm²
1.43 - 4760 ft-lb/in²
Average value: 0.664 J/cm² Grade Count:161
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.200 - 1000 J/cm²
0.952 - 4760 ft-lb/in²
Average value: 1.11 J/cm² Grade Count:124
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.600 - 1000 J/cm²
2.86 - 4760 ft-lb/in²
Average value: 2.75 J/cm² Grade Count:13
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Charpy Impact, Notched 0.200 - 1000 J/cm²
0.952 - 4760 ft-lb/in²
Average value: 1.55 J/cm² Grade Count:16
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.400 - 1000 J/cm²
1.90 - 4760 ft-lb/in²
Average value: 3.09 J/cm² Grade Count:31
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.100 - 1000 J/cm²
0.476 - 4760 ft-lb/in²
Average value: 1.21 J/cm² Grade Count:161
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.370 - 1000 J/cm²
1.76 - 4760 ft-lb/in²
Average value: 2.01 J/cm² Grade Count:64
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Charpy Impact, Notched 0.420 - 1000 J/cm²
2.00 - 4760 ft-lb/in²
Average value: 0.770 J/cm² Grade Count:5
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 1.00 - 1000 J/cm²
4.76 - 4760 ft-lb/in²
Average value: 2.00 J/cm² Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Charpy Impact, Notched 0.300 - 1000 J/cm²
1.43 - 4760 ft-lb/in²
Average value: 3.31 J/cm² Grade Count:11
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Charpy Impact, Notched 3.00 - 1000 J/cm²
14.3 - 4760 ft-lb/in²
Average value: 6.73 J/cm² Grade Count:48
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Charpy Impact, Notched 5.00 - 1000 J/cm²
23.8 - 4760 ft-lb/in²
Average value: 7.00 J/cm² Grade Count:13
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Charpy Impact, Notched 0.200 - 1000 J/cm²
0.952 - 4760 ft-lb/in²
Average value: 0.766 J/cm² Grade Count:239
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Charpy Impact, Notched 0.200 - 1000 J/cm²
0.952 - 4760 ft-lb/in²
Average value: 0.300 J/cm² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Charpy Impact, Notched 0.130 - 1000 J/cm²
0.619 - 4760 ft-lb/in²
Average value: 4.67 J/cm² Grade Count:31
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.300 - 1000 J/cm²
1.43 - 4760 ft-lb/in²
Average value: 1.82 J/cm² Grade Count:181
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..