Overview of materials for Nylon 6, Extruded

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 6, Extruded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.03 - 1.29 g/cc
0.0372 - 0.0466 lb/in³
Average value: 1.13 g/cc Grade Count:91
Water Absorption 0.0200 - 10.0 %
0.0200 - 10.0 %
Average value: 1.94 % Grade Count:45
Moisture Absorption at Equilibrium 1.30 - 3.00 %
1.30 - 3.00 %
Average value: 2.63 % Grade Count:33
Water Absorption at Saturation 8.50 - 10.0 %
8.50 - 10.0 %
Average value: 9.45 % Grade Count:31
Water Vapor Transmission 35.0 g/m²/day
2.25 g/100 in²/day
Average value: 35.0 g/m²/day Grade Count:16
992 - 992 g/m²/day

@Temperature 38.0 - 38.0 °C
63.9 - 63.9 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 992 g/m²/day Grade Count:1
Oxygen Transmission 1.00 - 1.95 cc-mm/m²-24hr-atm
2.54 - 4.95 cc-mil/100 in²-24hr-atm
Average value: 1.50 cc-mm/m²-24hr-atm Grade Count:16
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Average value: 40.3 cc/m²/day Grade Count:17
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
Average value: 14.0 cc-mm/m²-24hr-atm Grade Count:17
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
Average value: 72.8 cc-mm/m²-24hr-atm Grade Count:17
Viscosity 410000 - 2.25e+6 cP

@Temperature 260 - 260 °C
410000 - 2.25e+6 cP

@Temperature 500 - 500 °F
Average value: 888000 cP Grade Count:16
220 - 3.50e+6 cP

@Temperature 240 - 280 °C
220 - 3.50e+6 cP

@Temperature 464 - 536 °F
Average value: 888000 cP Grade Count:19
220 - 3.50e+6 cP

@Shear Rate 0.100 - 1000 1/s
220 - 3.50e+6 cP

@Shear Rate 0.100 - 1000 1/s
Average value: 888000 cP Grade Count:19
Viscosity Test 75.0 - 245 cm³/g
75.0 - 245 cm³/g
Average value: 205 cm³/g Grade Count:20
Maximum Moisture Content 0.0800
0.0800
Average value: 0.0800 Grade Count:17
Thickness 50.0 microns
1.97 mil
Average value: 50.0 microns Grade Count:16
Linear Mold Shrinkage 0.00127 - 0.0206 cm/cm
0.00127 - 0.0206 in/in
Average value: 0.0106 cm/cm Grade Count:18
Linear Mold Shrinkage, Transverse 0.00110 - 0.0207 cm/cm
0.00110 - 0.0207 in/in
Average value: 0.00514 cm/cm Grade Count:5
Melt Flow 1.10 - 22.7 g/10 min
1.10 - 22.7 g/10 min
Average value: 3.63 g/10 min Grade Count:24
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85.0
85.0
Average value: 85.0 Grade Count:3
Hardness, Rockwell R 97.0 - 121
97.0 - 121
Average value: 112 Grade Count:9
Ball Indentation Hardness 50.0 - 160 MPa
7250 - 23200 psi
Average value: 132 MPa Grade Count:5
Tensile Strength, Ultimate 42.0 - 80.0 MPa
6090 - 11600 psi
Average value: 71.4 MPa Grade Count:12
Film Tensile Strength at Yield, MD 30.0 - 40.0 MPa
4350 - 5800 psi
Average value: 32.2 MPa Grade Count:22
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
Average value: 30.0 MPa Grade Count:6
Tensile Strength, Yield 29.0 - 186 MPa
4210 - 27000 psi
Average value: 68.8 MPa Grade Count:40
Film Elongation at Break, MD 310 - 359 %
310 - 359 %
Average value: 346 % Grade Count:22
Film Elongation at Break, TD 280 - 360 %
280 - 360 %
Average value: 320 % Grade Count:5
Elongation at Break 1.50 - 315 %
1.50 - 315 %
Average value: 99.3 % Grade Count:40
Elongation at Yield 2.50 - 92.0 %
2.50 - 92.0 %
Average value: 11.7 % Grade Count:14
Modulus of Elasticity 0.350 - 3.50 GPa
50.8 - 508 ksi
Average value: 1.45 GPa Grade Count:44
Flexural Yield Strength 28.0 - 276 MPa
4060 - 40000 psi
Average value: 92.9 MPa Grade Count:32
Flexural Modulus 0.520 - 13.8 GPa
75.4 - 2000 ksi
Average value: 2.82 GPa Grade Count:27
Izod Impact, Notched 0.300 - 5.30 J/cm
0.562 - 9.93 ft-lb/in
Average value: 1.17 J/cm Grade Count:27
Izod Impact, Notched (ISO) 5.00 - 100000 kJ/m²
2.38 - 47600 ft-lb/in²
Average value: 18.1 kJ/m² Grade Count:11
3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.67 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) >= 100 kJ/m²

@Temperature -30.0 - -30.0 °C
>= 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 100 kJ/m² Grade Count:1
Charpy Impact Unnotched 12.5 J/cm² - NB
59.5 ft-lb/in² - NB
Average value: 18.9 J/cm² Grade Count:15
27.0 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
128 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 27.0 J/cm² Grade Count:3
Charpy Impact, Notched 0.300 - 1000 J/cm²
1.43 - 4760 ft-lb/in²
Average value: 3.31 J/cm² Grade Count:11
0.300 - 7.00 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 33.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.82 J/cm² Grade Count:4
Coefficient of Friction 0.0400 - 1.20
0.0400 - 1.20
Average value: 0.791 Grade Count:19
Coefficient of Friction, Static 1.20 - 1.50
1.20 - 1.50
Average value: 1.34 Grade Count:15
Tear Strength Test 0.500 - 33.0
0.500 - 33.0
Average value: 28.7 Grade Count:18
Tear Strength, Total 2070 - 3530 N
465 - 794 lb (f)
Average value: 2560 N Grade Count:6
Elmendorf Tear Strength MD 60200 - 115000 g
60200 - 115000 g
Average value: 85500 g Grade Count:6
Elmendorf Tear Strength TD 54000 - 116000 g
54000 - 116000 g
Average value: 89700 g Grade Count:6
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Average value: 88.0 MPa Grade Count:22
Film Tensile Strength at Break, TD 60.0 - 100 MPa
8700 - 14500 psi
Average value: 80.0 MPa Grade Count:5
Thermal Properties Metric English Comments
CTE, linear 19.8 - 170 µm/m-°C
11.0 - 94.4 µin/in-°F
Average value: 88.1 µm/m-°C Grade Count:36
CTE, linear, Transverse to Flow 70.0 - 190 µm/m-°C
38.9 - 106 µin/in-°F
Average value: 118 µm/m-°C Grade Count:5
Specific Heat Capacity 1.55 - 2.55 J/g-°C
0.370 - 0.609 BTU/lb-°F
Average value: 1.89 J/g-°C Grade Count:17
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+10 - 1.00e+16 ohm-cm
1.00e+10 - 1.00e+16 ohm-cm
Average value: 8.39e+14 ohm-cm Grade Count:20
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 8.03e+14 ohm Grade Count:15
Dielectric Constant 2.50 - 20.0
2.50 - 20.0
Average value: 4.47 Grade Count:14
Dielectric Strength 13.0 - 100 kV/mm
330 - 2540 kV/in
Average value: 28.4 kV/mm Grade Count:20
Dissipation Factor 0.00580 - 0.120
0.00580 - 0.120
Average value: 0.0361 Grade Count:9
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:8