Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.619 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.130 - 0.200 J/cm²
0.619 - 0.952 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Charpy Impact, Notched 0.130 - 0.150 J/cm²
0.619 - 0.714 ft-lb/in²
Injection and Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Charpy Impact, Notched 0.130 - 1.70 J/cm²

@Temperature -30.0 - 10.0 °C
0.619 - 8.09 ft-lb/in²

@Temperature -22.0 - 50.0 °F
Average value: 0.367 J/cm² Grade Count:85
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.130 J/cm²

@Temperature 23.0 °C
0.619 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free  (discontinued **)
Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy..
Charpy Impact, Notched 0.130 J/cm²

@Temperature 23.0 °C
0.619 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications..
Charpy Impact, Notched 0.130 - 0.530 J/cm²
0.619 - 2.52 ft-lb/in²
Average value: 0.363 J/cm² Grade Count:6
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
LATI Latigray 52/11-01 CX/70 PP Homopolymer
Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
ISO 179-1
Vyncolit TX10916 Graphite Filled Novolac Phenolic
Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc.
Charpy Impact, Notched 0.130 J/cm²

@Temperature -30.0 °C
0.619 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 3248 TC Polypropylene
Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
DIN 53453
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
LATI Latimass 52/11-01 D020 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
LATI Latimass 52/11-04 D008 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
LATI Latimass 52/35-04 D009 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Charpy Impact, Notched 0.130 J/cm²
0.619 ft-lb/in²
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Charpy Impact, Notched 0.130 - 1000 J/cm²
0.619 - 4760 ft-lb/in²
Average value: 4.67 J/cm² Grade Count:31
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Copyright © lookpolymers.com All Rights Reserved