| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded |
| Manufacturer | LG Chemical |
| Trade Name | LUPOY |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical LUPOY GP1000M PC, Transparent.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0080 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 11 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
11 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength, Yield | 61.8 MPa <br>@Thickness 3.20 mm |
8960 psi <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | >= 150 % <br>@Thickness 3.20 mm |
>= 150 % <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 98.1 MPa <br>@Thickness 3.20 mm |
14200 psi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Flexural Modulus | 2.26 GPa <br>@Thickness 3.20 mm |
327 ksi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Izod Impact, Notched | >= 7.35 J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
>= 13.8 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 130 °C <br>@Thickness 6.40 mm |
266 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 141 °C <br>@Load 5.00 kg |
286 °F <br>@Load 11.0 lb |
50°C/h; ASTM D1525 |
| UL RTI, Electrical | 130 °C <br>@Thickness >=1.50 mm |
266 °F <br>@Thickness >=0.0591 in |
|
| 130 °C <br>@Thickness >=3.00 mm |
266 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 130 °C <br>@Thickness >=1.50 mm |
266 °F <br>@Thickness >=0.0591 in |
|
| 130 °C <br>@Thickness >=3.00 mm |
266 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 130 °C <br>@Thickness >=1.50 mm |
266 °F <br>@Thickness >=0.0591 in |
|
| 130 °C <br>@Thickness >=3.00 mm |
266 °F <br>@Thickness >=0.118 in |
||
| Flammability, UL94 | HB <br>@Thickness >=1.50 mm |
HB <br>@Thickness >=0.0591 in |
|
| HB <br>@Thickness >=3.20 mm |
HB <br>@Thickness >=0.126 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
| Dielectric Strength | 17.0 kV/mm <br>@Thickness 1.00 mm |
432 kV/in <br>@Thickness 0.0394 in |
ASTM D149 |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D492 |
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
| Hot Wire Ignition, HWI | 30 - 60 sec <br>@Thickness >=1.50 mm |
30 - 60 sec <br>@Thickness >=0.0591 in |
|
| 60 - 120 sec <br>@Thickness >=3.00 mm |
60 - 120 sec <br>@Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | >= 120 arcs <br>@Thickness 1.50 mm |
>= 120 arcs <br>@Thickness 0.0591 in |
|
| >= 120 arcs <br>@Thickness 3.00 mm |
>= 120 arcs <br>@Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
| Middle Barrel Temperature | 255 - 280 °C | 491 - 536 °F | Injection Molding |
| Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
| Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
| Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | Injection Molding |
| Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
| Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
| Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |